| Silicone | Acrylic | Polyurethane | |
|---|---|---|---|
| Cure mechanism | Moisture cure | Water evaporation | Chemical cure |
| Ponding water resistance | High — unaffected by standing water | Low — softens and can re-emulsify | Moderate to high |
| UV stability | Excellent — strongest of the three | Good, chalks over time | Aromatic grades degrade; aliphatic topcoat required |
| Abrasion and traffic resistance | Lower — slippery when wet | Moderate | Highest of the three |
| Dirt pickup | Higher — reflectance declines faster | Lower | Moderate |
| Recoating at end of term | Requires specific preparation to re-adhere | Straightforward | Straightforward |
| Best suited to | Roofs with imperfect drainage, high UV exposure | Well-drained roofs, budget restorations | High-traffic roofs, mechanical rooms, walkways |
Restoration is viable when
Replacement is required when
1
Infrared, capacitance metering, or core cuts establish substrate moisture. A test patch confirms the coating adheres to the existing membrane, which varies by membrane type, age, and prior coating history. Both results precede any specification.
2
The roof is power washed to remove dirt, chalk, biological growth, and residue. Adhesion failure most often traces to a surface that was coated before it was clean. Amarillo's airborne dust makes the rinse and dry stage as consequential as the wash.
3
Splits, open seams, blisters, and failed flashings are repaired before coating. A coating spans a hairline crack; it does not bridge an open seam or a deteriorated flashing.
4
Polyester reinforcing fabric is embedded in coating at seams, penetrations, curbs, drains, and transitions. Reinforced details carry movement that a bare film cannot. This stage is where restoration systems are either built to last or built to fail on schedule.
5
Base and top coats applied by spray or roller to the specified dry film thickness, verified by wet mil gauge during application rather than estimated afterward. Silicone is high-solids, so wet and dry film readings track closely.
6
Warranty term is a direct function of applied dry film thickness. Manufacturers publish the relationship, and the specification should state the thickness rather than only the warranty year.
10-year term. Suited to shorter ownership horizons and budget-constrained restorations. Thin film in a high-UV market reaches the end of serviceable life before the end of the warranty term.
15-year term — Velzen standard specification for Amarillo, TX. Film thickness is the reserve the coating draws on as the surface weathers under a UV index of 11.
20-year term. Long-hold assets, high UV exposure, and roofs with imperfect drainage where the film carries more work.
Where the moisture survey supports restoration, five advantages apply beyond the direct cost difference.
Velzen Roofing completes roof replacements within a 120-mile radius of Amarillo, TX — covering 15 cities across 13 Texas Panhandle counties with no additional travel fees inside the primary service area.
Frequently Asked Questions
Survey First
Ready to book your free roof inspection?
Call (806) 214-0055 and pick a time that works for you. Phone lines are open Monday to Friday, 8 AM to 6 PM.